Luoyang Magnesium Gurnee Metal Material Co.;Ltd
|
Price: | 30.0 USD |
Payment Terms: | T/T,L/C,D/A,D/P |
Place of Origin: | Henan, China (Mainland) |
Add to My Favorites | |
HiSupplier Escrow |
Nickel plate; nickel sheet; nickel strip
1).Material:Nickel
2).Standard:ASTM AMS,DMS,ASME,MIL
3).specification: Thick:0.1-100mm,Width:100-2500mm,Length:1m,2m,6m or can be customerized
4).Characteristic:high specific strength,excellent processability and decoration,Unique corrosion
resistance,Light weight, High strength,High performance and so forth
5).Condition:good
6) .Delivery time:7days~15days
7).packing details:wooden case outside soft paper inside.
8). As per GB, ASTM standard, we can supply nickel plate, bar,tube, wire and related nickel alloy products
with various types.
Nickel plate Physical properties
Density | 8.1 g/cm³ |
Melting point | 1320-1390 °C |
Nickel plate Chemical composition
Alloy | % | Ni | Cr | Fe | Mo | C | Mn | Si | Cu | Al | Ti |
926 | Min. | 24 | 19 | balance | 6.0 | 0.2 | 0.6 | ||||
Max. | 26 | 21 | 7.0 | 0.08 | 0.35 | 0.5 | 0.3 | 0.8 | 1.2 |
Nickel plate properties in the room temperature
Alloy | Tensile strength | Yield strength | Elongation | Brinell hardness HB |
Solution treatment | 650 | 295 | 35 | ≤363 |
Type | process | Delivery condition | diameter(mm) | standard |
N4,N5,N6,N7,N02200,N02201 | Hot rolled+ grounded | R M | 6-200 | GB4435 ASTM B160 DIN17740 |
NCu28-2.5-1.5, NCu40-2-1 | Hot rolled+ grounded |
Other information of Nickel Plate
Brand Property | Cr20Ni80 | Cr30Ni70 | Cr15Ni60 | Cr20Ni35 | Cr20Ni30 | |
Major chemical component% | Ni | Margin | Margin | 55.0-61.0 | 34.0-37.0 | 30.0-34.0 |
Cr | 20.0-23.0 | 28.0-31.0 | 15.0-18.0 | 18.0-21.0 | 18.0-21.0 | |
Fe | ≤1.0 | ≤1.0 | Margin | Margin | Margin | |
Component max. use temperature | 1200 | 1250 | 1150 | 1100 | 1100 | |
Melting Point | 1400 | 1380 | 1390 | 1390 | 1390 | |
Density g/cm3 | 8.40 | 8.10 | 8.20 | 7.90 | 7.90 | |
Resistivity μΩ·m,20 | 1.09±0.05 | 1.18±0.05 | 1.11±0.05 | 1.04±0.05 | 1.04±0.05 | |
Extension rate% | 20 | 20 | 20 | 20 | 20 | |
Specific Heat J/g. | 0.440 | 0.461 | 0.494 | 0.500 | 0.500 | |
Heat Conduction Coefficient KJ/M.h | 60.3 | 45.2 | 45.2 | 43.8 | 43.8 | |
Linear expansion coefficient aX10-6/ | 18.0 | 17.0 | 17.0 | 19.0 | 19.0 | |
Microstructure | Austenitic | Austenitic | Austenitic | Austenitic | Austenitic | |
Magnetic | Non-magnetic | Non-magnetic | Non-magnetic | Non-magnetic | Non-magnetic |